: Thank you Mike,
: I sanded and coated once... Looks much better already! BTW, for the
: sake of any future builders the Rustoleum professional flat
: black has limestone in the formula and I think might be the
: culprit in the cracking finish.
: Cheers!

Flat black is part of the problem here, can't reflect any of the sun's rays and will heat up more than any other color. UV and heat are causing the paint to break down.

Bill H.

Messages In This Thread

Skin-on-Frame: Rustoleum "professional" hairline cracks/pinholes *PIC*
Miami Tavo -- 7/19/2012, 4:50 pm
Re: Skin-on-Frame: Rustoleum "professional" hairli
Mike Savage -- 7/20/2012, 6:00 am
Re: Skin-on-Frame: Rustoleum "professional" hairli
Miami Tavo -- 7/20/2012, 6:51 am
Re: Skin-on-Frame: Rustoleum "professional" hairli
Mike Savage -- 7/21/2012, 7:15 am
Re: Skin-on-Frame: Rustoleum "professional" hairli
Miami Tavo -- 7/22/2012, 1:37 pm
Re: Skin-on-Frame: Rustoleum "professional" hairli
Bill Hamm -- 7/23/2012, 1:20 am
Re: Skin-on-Frame: Rustoleum "professional" hairli
Mike Savage -- 7/23/2012, 7:49 am
Re: Skin-on-Frame: Rustoleum "professional" hairli
Miami Tavo -- 7/24/2012, 8:04 pm