Here’s my and my brother’s latest debate: How much fiberglass does a C16 S&G need if door skins are used for plywood.

Me, I’m paranoid. I want at least 6oz on the bottom and 4oz on the top.
Brother wants to go down to 2oz on the bottom and none on the top.
We both thinking fiberglass tape only on the inside seams.

Your opinions please.
Roger Nuffer

Messages In This Thread

To glass or not to glass. That's the S&G ?
Roger Nuffer -- 7/25/2001, 1:26 am
on one hand -- and then again, on the other hand
Paul G. Jacobson -- 7/25/2001, 3:09 am
Re: on one hand -- and then again, on the other ha
Roger Nuffer -- 7/25/2001, 3:49 am
Re: on one hand -- and then again, on the other ha
Bob Kelim -- 7/25/2001, 11:39 pm
Re: on one hand -- and then again, on the other ha
Bill Price -- 7/25/2001, 1:20 pm
Re: Multiple Layers
Mike Hanks -- 7/25/2001, 10:43 am