Re: fumed silica

Posted By: Shawn Baker
Date: Friday, 12 November 1999, at 10:15 a.m.

In Response To: fumed silica (Tom Kurth)

Yep, same stuff. Also sold as Cab-o-Sil or Cabosil. It is a thixotropic (non-sag) agent that you can add to epoxy to make it thicker and resistant to running out of a joint. It can also help make an epoxied joint stronger because it keeps the joint halves separated slightly so they're not "resin-starved".

Works great. It's super fine stuff--you probably don't want to breathe the stuff in, though.

Does anyone know if silica fume would cause silicosis?

Shawn

> While looking over literature from our fiberglass supplier at work, I came
> across the item "fumed silica." Does anybody know if this is the
> same as colloidal silica? Does anybody know its use? Thanks, Tom

Messages In This Thread

fumed silica
Tom Kurth -- Thursday, 11 November 1999, at 9:44 p.m.
Re: fumed silica
Shawn Baker -- Friday, 12 November 1999, at 10:15 a.m.
Re: colloidal silica - handling precautions
Michael Freeman -- Friday, 12 November 1999, at 5:37 p.m.

[ View Thread ] [ Return to Index ] [ Read Prev Msg ] [ Read Next Msg ]

KBBS Archive 10,000 is maintained by Nick Schade - Guillemot Kayaks with WebBBS 5.12.

 Guillemot | SEE Kayak Directory | Kayak Forum

The Kayak Forum is Sponsored By

Guillemot Kayaks

Guillemot Kayaks